Molecular SieveZeolite AdsorbentsBy SorbiTech™
Pile of white desiccant beads on a steel bench

Molecular Sieve Insulating Glass Desiccant

A free flowing 3A bead for spacer bar filling that keeps the cavity dry and the argon fill in place.

Find My Solution

Quick Answer

Insulating glass desiccant keeps the sealed cavity of a double glazed unit dry. A molecular sieve 3A bead in the spacer bar takes up water vapour, while argon and nitrogen are too wide for its 3 Å pore. The gas fill and the insulation value therefore stay in the unit for its working life.

  • Molecular sieve 3A
  • IG 3A beads
  • 13X and 3A blends for solvent seals
  • Packing density by ASTM D4164
  • Manufactured by Medaad

Request the TDS Request the SDS

Updated

Moisture in a Sealed Cavity

An insulating glass unit is two panes held apart by a hollow spacer bar and closed with a seal system. The cavity between them is sealed at the factory and never opened.

It still takes up moisture. No seal stops water vapour completely, so over the years the cavity gains water. When the outside temperature drops far enough, that water condenses on the inner face of the glass.

Argon Fill and Pane Deflection

A desiccant with a wider pore can take up nitrogen, oxygen and argon as well as water. That lowers the pressure in the sealed cavity. The panes are pulled towards each other and the unit deflects. On a large pane this shows as a distorted reflection, and the seal takes the load.

A 3 Å window keeps all three gases out, so the grade for this duty is 3A.

Figure 01 · A unit in section
PANEPANESPACER, FILLED WITH 3ASEAL SYSTEMSEALED CAVITYAIR OR ARGONWATER IN HELD BY THE BEADFILL GAS MUST NOT BE HELDSEAL SOLVENT HELD BY A BLENDThree things reach it. Two should stick.

Figure 01 · Arrangement only, not to scale. Spacer depth and seal thickness vary with the system.

In the cavityMoleculeInto a 3 A pore
Water vapour2.6 angstromyes, the duty
Oxygen3.5 angstromno
Argon fill3.4 angstromno
Nitrogen3.6 angstromno

Seal Solvent and 13X Blends

A polysulfide or polyurethane secondary seal gives off solvent vapour as it cures. The vapour stays in the cavity.

If the desiccant cannot hold it, it condenses as a haze on the inside of the glass that cannot be cleaned off. Units with these seals are filled with a blend of 13X and 3A. The 13X takes the solvent.

Fogging and Deflection Complaints

Condensation means the desiccant ran out of capacity, or there was too little in the bar. The fix is more desiccant or a better seal.

Deflection means the desiccant took up the fill gas. The fix is a narrower pore grade.

ComplaintWhat it meansWhat changes
Condensation on the glasscapacity ran outmore desiccant, or a better seal
Haze that will not clean offseal solvent condenseda blend that holds solvent
Panes pulled inwardthe fill gas was adsorbeda narrower grade
Early failure across a batchdesiccant exposed before fillingbetter handling

Filling the Spacer Bar

The bead goes into the hollow bar through fill holes, usually on an automatic filler in line with production.

The bead must flow freely, so it is round and of uniform size. It must also be kept sealed until use. Desiccant left open to factory air takes up water and loses capacity before the unit is closed.

IG 3A and Blended Grades

SorbiTech supplies IG 3A, a bead made for this duty, and blended grades for solvent based seal systems.

The sealant decides which one a line needs. Grade selection covers the choice in general.

Seal systemGrade for the spacer
Hot melt, no solvent releasedIG 3A
Polysulfide or polyurethane, solvent released on curing13X and 3A blend

Supply to Glazing Lines

Glazing lines buy on a regular schedule. Static desiccant packs for crates and enclosures are a separate duty, covered under static desiccant.

Request a Quote

Related Grade and Quality Pages

The base grade is described under 3A molecular sieve, and the wider pore grade in the blend under 13X molecular sieve. How an order specification is written is set out under quality. The desiccant beads are made by Medaad, the group manufacturer.

Insulating Glass Desiccant Questions

What should be checked when units fail in the field?

Desiccant handling and the seal system, before the grade is changed.

How is the bead packed for a filling line?

In sealed packaging sized to a filling machine hopper, so the bead stays dry until it goes into the bar.

How is the quality of a delivery specified?

Each order carries a specification that names the properties, their limits and the test methods. For a spacer bead, residual water as packed is a useful line. It is measured by loss on heating at a temperature stated in the specification.

How are fines from the bead measured?

Attrition loss by ASTM D4058 measures the fines particles produce when they rub together. Low fines keep the filler running and the spacer holes clear.

Who makes IG 3A and the blended grades?

Medaad, the group manufacturer, makes both. SorbiTech supplies them to glazing lines.

Quote for Insulating Glass Desiccant

Tell us the sealant system, hot melt or solvent based, with the spacer profile and the annual volume.

Request a Quote
Contact
Email[email protected] Call+971 56 777 3027