Molecular Sieve Loading and Replacement

When a charge is spent, and how a change out runs from unloading to the dry out.

Related Solutions

Quick Answer

A molecular sieve charge is due for replacement when the bed can no longer hold the outlet dew point for its full adsorption time, or when pressure drop or dust makes it unworkable. A change out then removes the spent sieve safely, renews the support media where needed, loads the new charge from the grid upward and dries it before start up.

  • ASTM D4164 tapped density
  • ASTM D4058 attrition loss
  • 25 kg and 150 kg drums, 850 kg big bags

Request the TDS Request the SDS

Engineering GuideUpdated

The decision is based on plant data. Most charges in oil and gas processing are replaced at a planned shutdown. The steps below follow common industry practice and are given for guidance. The site's own permits, isolation and vessel entry rules govern every step.

Signs a Molecular Sieve Charge Is Spent

Four signals show that a charge is nearing its end.

  • Outlet moisture. Water content at the end of each adsorption step creeps up, and the dew point starts to rise earlier in the cycle.
  • Shorter breakthrough. To hold specification, operators shorten the adsorption time. Once the shortened step no longer covers the heating and cooling time of the other towers, the bed is spent.
  • Rising pressure drop. A steady climb across the bed points to broken beads, caking or fouling in the packing.
  • Dust downstream. Fines on outlet filters, valves or exchangers show beads breaking up. The causes are covered in molecular sieve lifetime and dusting.

A breakthrough test turns the trend into a number. A portable hygrometer is connected to the outlet of the oldest bed, and the time from the start of adsorption to a steady rise in dew point is recorded. Repeating the test on each tower shows how much working capacity remains. In gas plants that recover natural gas liquids, capacity commonly decays by about 5 to 15 percent a year, so one test plus the design margin gives a fair estimate of the months left. In natural gas dehydration ahead of LNG liquefaction plants, rising pressure drop at the cold box can be the first hint that water is passing.

Change Out Planning Sequence

The table sets out a typical sequence.

StepWhat is doneWhy
Confirm the needBreakthrough tests, pressure drop and filter trends reviewedAvoids replacing a charge with life left, or running one past its end
Define the chargeGrade, bead size, layer heights and ball sizes checked against the vessel drawing and the original bed designA wrong bead or ball size shows up later as pressure drop or lost beads
Order and storeNew sieve, balls and screens ordered against an agreed specification and kept sealed and dryOpen sieve takes up moisture from the air
Prepare the vesselFinal regeneration, cooling, depressuring, blinding and nitrogen purgeStrips as much adsorbed material as possible before opening
Unload and inspectSpent sieve removed, grid, screens, wall seal and thermowells inspectedDamaged internals cause bypass or bead loss in the next run
Dry out and startDust purge, full regeneration, slow pressurisingRemoves water picked up while the vessel was open

The steps are the same whether the vessel holds 3A molecular sieve for syngas and ammonia drying, 4A molecular sieve for LPG and NGL treating, or 13X molecular sieve in air prepurification. A change out is also a good time to review the grade, using molecular sieve types and how to choose between them. Pack format affects the lifting plan. Sieve from Medaad, which makes the group's adsorbents, comes in 25 kg and 150 kg drums and 850 kg big bags, as described under molecular sieve manufacturing.

Unloading Spent Sieve Safely

Spent sieve can still hold hydrocarbons, H₂S, mercaptans or other process residues after a final regeneration. It is treated as hazardous until the residues are known. The usual preparation is to regenerate once more, cool fully, depressure, fit blind flanges and purge with nitrogen until the vessel is free of process gas. Where a nitrogen purge was used, the blanket is held while the sieve is dumped.

  • Toxic and flammable gas. Fumes can be released as the bed is disturbed. Breathing apparatus and fire water stay on standby, and dumping stops if the material starts to burn or heat up.
  • Heat on contact with water. Active sieve releases strong heat when wetted. If a bed is quenched, the water needed just to wet it is about half the weight of the sieve, with more to absorb the heat, and the vessel and supports must carry that extra weight.
  • Dust. Crews wear eye protection, dust masks, gloves, safety shoes and clothing that covers the body.
  • Confined space. Nobody enters the vessel while sieve remains inside, and later entry follows the site's confined space rules.

Sieve is normally drained through a bottom dump nozzle or manway, or vacuumed into closed containers. In sour gas dryers and mercaptan removal beds, the sulfur load makes these precautions especially important.

Support Balls and Screens

The bed rests on a steel grid covered by wire screen with openings of about 1 mm. The screen is cut a little smaller than the vessel and sealed at the wall, so it can move with heat without letting beads past. Before anything is loaded, crews check that seal, clear old beads out of the screen and mark each layer height on the vessel wall. Figure 1 shows the order in which the layers go in.

Figure 01 · Section through a dryer vessel, filled from the support grid upward
FLOW INTOP BALLSMOLECULARSIEVESMALL BALLSLARGE BALLSHOLD DOWN, 13 MM, 100 MM OR MOREFLOATING SCREENSOCK OR DENSE LOADEDSHORT FREE FALL6 MM, 75 MM OR MORE13 MM, 75 MM OR MORESCREEN ON SUPPORT GRIDLOADED LASTLOADING ORDERLOADED FIRST

Ball sizes and layer depths are typical values from published loading practice, for guidance only. Layer heights are not to scale.

Graded inert balls sit on the screen, at least 150 mm in total. A common layout starts with 13 mm balls and then 6 mm balls, each size about half the one below, until the top layer is roughly twice the sieve bead size. Each layer is commonly at least 75 mm deep. The balls spread the flow at the outlet and keep beads off the screen. They are lowered gently, because balls dropped from the top can shatter and tear the screen. Any unloading nozzle is filled with support media before the sieve goes in. Grid, distributor and nozzle details belong to adsorber vessel design.

Sock Loading and Dense Loading

In sock loading, drums or big bags are emptied into a hopper lifted just above the top manway. The sieve runs down a canvas sock to the bed surface. A crew member moves the sock across the vessel so no cone forms, and each lift is levelled with a plank. Published loading guidance limits free fall from the sock end to about 7 to 10 metres, because longer drops break beads and make dust.

Dense loading uses a spreader at the manway that throws beads evenly across the whole cross section. Each bead lands on its own and settles flat, so the bed packs closer. More sieve fits in the same vessel, and the bed settles less once in service. The trade is a higher pressure drop per metre of bed, so dense loading is decided at the design stage. Pneumatic transfer from a truck is quick but rough on the beads. In one published trial about 2.5 percent of the charge came out as fines and dust.

Levelling and the Hold Down Layer

Once the sieve reaches its mark, the surface is levelled. An uneven top lets gas take the short path through the thin side, and that side breaks through first. A floating screen goes on the sieve, free to move as the bed expands and shrinks with each heating cycle. A hold down layer of inert balls sits on top, commonly at least 100 mm of 13 mm balls. Its weight keeps beads from lifting and swirling in the inlet flow, a major source of attrition.

A clear space of about 90 cm or more is left between the inlet nozzle and the top balls. Where the inlet has no proper distributor, the top ball layer is often deepened to about 150 mm to break the jet. The large adsorbers of air separation plants meet the same aims with their own internals. All packaging, liners and loading gear are removed before the manways close. The vessel is then closed with new gaskets and leak tested before any process gas is admitted.

Dry Out and Start Up of a New Charge

New sieve picks up moisture from the air while the vessel stands open. The first step after closing is a purge with dry nitrogen or dry gas, run from top to bottom through the outlet filters, to carry loose dust away.

The charge then receives a full regeneration before it goes on line. Values for that first heat, the hold and the cooling end point are set out in molecular sieve regeneration temperature and cycle. Pressure is raised slowly so the fresh bed does not lift. A small temperature rise is normal as the sieve meets the feed, but a large one calls for the feed to be stopped. Once each bed has completed one adsorption step without an unusual rise, the unit is ready for normal service. In olefin plants the bed is often preloaded with a little olefin during cooling, so the heat of first contact is spread out, a step that belongs to cracked gas and olefin drying.

Questions on Change Out and Loading

How long does a molecular sieve change out take?

It depends on vessel size, access, the sulfur or hydrocarbon load on the spent sieve and the pack format. Purging and cooling before the vessel is opened often take longer than the unloading itself. On a dehydration unit with three or more towers, towers can sometimes be changed one at a time while the others keep running, if the plant can accept reduced throughput.

Can old support balls be reused?

Often they can, if they are intact, clean and the right size. Balls are screened and inspected after unloading. Chipped or cracked balls, and balls coated with fines, coke or sulfur, are better replaced, because they raise pressure drop and can let sieve reach the screen. Many plants renew at least the top hold down layer, which takes the most wear from the inlet flow.

Does dense loading matter for a small dryer?

Less so. In small vessels such as compressed air dryers or refrigerant drying cartridges, careful pouring and light tapping give a firm bed. The aim is the same as in a large vessel, a level bed with no voids where gas can bypass. Dense loading equipment pays off mostly in large gas plant vessels.

What should be done with spent molecular sieve?

Disposal follows local regulations, and the route depends on what the sieve held. The zeolite itself is an aluminosilicate, chemically close to ordinary clay, so the residues decide how it is classed. A laboratory analysis of a sample usually settles that question. Sieve from refinery or sour service often has to be handled as industrial waste, so the local authority should be consulted before the shutdown.

How should new molecular sieve be stored before loading?

Sealed in its original packs, indoors or under a waterproof cover, and off the ground on pallets. Big bags suit only short outdoor storage of a few weeks. A damaged pack is resealed at once, kept apart and tested for activity before use. Why open sieve takes up water so fast is explained in what a molecular sieve is.

Request a Quote for a Replacement Charge

To plan a replacement charge, send SorbiTech the vessel diameter and each layer height, the grade and bead size now in service, the support ball sizes and the date of the last change out. Recent dew point readings and breakthrough times, the pack format the site can lift and the shutdown date complete the picture. The specification is agreed for each order.

Request a Quote
Contact
Email[email protected] Call+971 56 777 3027